This linear polyesters produced in nature by bacterial fermentation of sugar or lipids
-
For Injection Molding
-
ASTM standards require testing of plastic samples in a simulated marine environment for six months while at 30 degree Celsius
-
This plastic resin made samples passed the biodegradation of ASTM D7081 by converting more than 30% of the carbon in the sample to CO2 within 180 days
-
The report were not found to contain any hazardous byproducts after 180 days of exposure to marine water through testing with FTIR, ATR FTIR, and DSC
-
This material did not release any detectable toxic chemicals into the marine water after 180 days